da Mafi kyawun Superalloy Inconel625/ UNS N06625Guojin

Superalloy Inconel625/ UNS N06625/ Mai ƙera Alloy625

Takaitaccen Bayani:

Daidai da daraja:
Bayanan N06625
DIN W. Nr.2.4856


Cikakken Bayani

Tags samfurin

Samfuran Samfura

Bututu mara nauyi, Faranti, Sanda, Forgings, Fasteners, Kayan aikin bututu

Ka'idojin samarwa

Samfura

ASTM

Bar

B446

Plate, Sheet da Strip

B 443, B 906

Bututu mara kyau, tube

B 444, B 829

Bututu mai walda

B 705, B 775

Kayan aikin walda

B 704, B 751

Welded connectors

B366

Ƙirar ƙirƙira da sanduna

B472

Ƙirƙira

B564

Haɗin Sinadari

%

Ni

Cr

Mo

Fe

C

Mn

Si

P

S

Co

Nb+Ta

Al

Ti

Min

58.0

20.0

8.0

3.15

Max

23.0

10.0

5.0

0.10

0.50

0.50

0.015

0.015

1.00

4.15

0.40

0.40

Abubuwan Jiki

Yawan yawa

8.36g/cm3

Narkewa

1330-1375 ℃

Inconel 625 Features

1. Kyakkyawan juriya na lalatawa ga kafofin watsa labaru daban-daban masu lalata a cikin oxidizing da rage yanayin
2. Kyakkyawan juriya ga pitting lalata da lalata lalata, kuma ba zai haifar da lalatawar damuwa na chloride ion ba.
3. Kyakkyawan juriya ga inorganic acid, kamar nitric acid, phosphoric acid, sulfuric acid, hydrochloric acid da gauraye acid na sulfuric acid da hydrochloric acid, da dai sauransu.
4. Kyakkyawan juriya ga lalata daban-daban inorganic acid gauraye mafita
5. Lokacin da yawan zafin jiki ya kai 40 ℃, zai iya nuna mai kyau lalata juriya a daban-daban yawa na hydrochloric acid bayani.
6. Good workability da weldability, babu post-weld fatattaka hankali
7. Manufacture takardar shaida na matsa lamba tasoshin da bango zafin jiki na -196 ~ 450 ℃
8. Ƙwararrun Ƙwararrun Injiniyan Lantarki ta Amirka NACE misali (MR-01-75) don saduwa da mafi girman matakin VII don amfani a cikin mahallin gas mai tsami.

Inconel625 Yankunan Aikace-aikace

The softened da annealed low carbon gami 625 ana amfani da ko'ina a cikin sinadaran aiwatar masana'antu, da kuma ta mafi lalata juriya da babban ƙarfi taimaka shi da za a yi amfani da a matsayin siriri tsarin bangaren.Ana iya amfani da Alloy 625 a cikin aikace-aikacen da aka fallasa zuwa ruwan teku da kuma batun babban damuwa na inji.Wuraren aikace-aikace na yau da kullun:
1. Abubuwan da ke tattare da tsarin sinadarai masu dauke da chlorides, musamman inda ake amfani da sinadarin chloride acid
2. Digesters da tankunan bleaching don masana'antar ɓangaren litattafan almara da takarda
3. Hasumiya mai shayarwa, reheater, bututun iskar gas mai hayaki, fan (humid), agitator, deflector da flue a cikin tsarin desulfurization flue gas
4. Don samar da kayan aiki da kayan aiki don amfani a cikin yanayin gas mai tsami
5. Acetic acid da acetic anhydride dauki janareta
6. Sulfuric acid condenser